posted on 20.12.2018, 13:28 authored by Stefania Marcotti, Damien LacroixDamien Lacroix, Gwendolen ReillyGwendolen Reilly
Pre-processed data obtained by AFM nano-indentation of MLO-A5 pre-osteocyte cells. The data pre-processing consisted in contact point fitting, tip-sample separation correction and drift correction of raw data, all performed in MATLAB (v2016a).

The experimental methodology and data processing are described in the author's thesis (Chapter 4).

Methods

* AFM cantilever preparation
Spherical tipped cantilevers were prepared. To increase the possibility of sensing the glycocalyx, softer cantilevers were chosen with nominal spring constant equal to 0.01 N/m (Windsor Scientific) and silica beads of different sizes were tested (D = 1; 2:5; 6 μm, Bangs Laboratories).

* AFM set-up
A NanoWizard 3 atomic force microscope (JPK Instruments AG) coupled to an Eclipse Ti-S optical inverted microscope (Nikon Instruments) was used for all the experiments.The cells were washed in phosphate buffer solution (PBS) and fresh medium was added. Samples were positioned on the heated sample holder to allow for testing at 37◦C.
Single cells were located through the coupled optical microscope and images of cell shape were recorded for morphological analysis. The cantilever was centred over the location of interest and a grid of 5 points spaced 3 μm within each other was set. Force spectroscopy measurements were obtained on the 5-point grid for 3 times to collect a total of 15 data on each location. The relative set point and the approach velocity were set to 10 nN and 4 μm/s respectively.

Funding

University of Sheffield ‘Mechanoreceptors in health and disease’ Network Scholarship

History

Ethics

There is no personal data or any that requires ethical approval

Policy

The data complies with the institution and funders' policies on access and sharing

Sharing and access restrictions

The data can be shared openly

Data description

  • The file formats are open or commonly used

Methodology, headings and units

  • Headings and units are explained in the files